Add to Cart
U Bend Return , ASTM A403 WP347H 180 Degree Elbow, Short Radius, Heat Exchanger , Boiler
Grade 347 is an austenitic stainless steel that is stabilized with niobium to enhance its resistance to intergranular corrosion. This stabilization makes it particularly effective in high-temperature environments (Excellent resistance to creep and stress rupture at elevated temperatures), where it exhibits excellent mechanical properties and corrosion resistance (Intergranular Corrosion Resistance, General Corrosion Resistance). Grade 347 is widely used in applications requiring high temperature and corrosion resistance, such as in the aerospace, chemical, and power generation industries.
High Temperature Performance:
Chemical Composition:
Grade | Ni | Cr | Fe | Si | C | Mn | P | S | Nb+Ta |
WP347 | 9-13% | 17-19% | Balance | 1% max | 0.08% max | 2% max | 0.045% max | 0.03% max | 10xC min to 1% |
Mechanical Properities:
Tensile Strength | Yield Strength | Elongation | Hardness |
Minimum 515 MPa (75,000 psi) | Minimum 205 MPa (30,000 psi) | Minimum 40% in 50 mm (2 inches) | Maximum 217 HB (Brinell hardness) |
Applications: