Extruded Fin Tube , ASTM B163 Incoloy 825 Base Tube , Fin Material Aluminum
Extruded fin tubes with a base tube made of ASTM B163 Incoloy are specialized components designed for high-performance heat transfer applications. Incoloy, a family of nickel-chromium-based superalloys, provides excellent resistance to oxidation, corrosion, and high-temperature environments, making it an ideal choice for demanding applications. And their excellent thermal performance, combined with the robust properties of Incoloy, makes them suitable for a wide range of high-temperature and corrosive applications across various industries.
Advantages :
1. High Thermal Efficiency:
2. Durability and Longevity:
3. Versatility:
Features of Extruded Fin Tubes with ASTM B163 Incoloy Base Tube:
Construction:
YUHONG GROUP Fin Tube Specification | |||||
Type | Description | Base tube | Fin specification (mm) | ||
O.D. (mm) | Fin Pitch | Fin Height | Fin Thick | ||
Extruded | Single Metal Combined Metal | 8-51 | 1.6-10 | <17 | 0.2-0.4 |
Low Fin tube t-type fin tube | 10-38 | 0.6-2 | <1.6 | ~0.3 | |
Bamboo tube corrugated tube | 16-51 | 8~30 | <2.5 | / |
Equivalent Material:
STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN | OR |
Incoloy 825 | 2.4858 | N08825 | NCF 825 | NA 16 | ЭП703 | NFE30C20DUM | NiCr21Mo | XH38BT |
Chemical Composition:
Element | Ni | Cr | Mo | Cu | Ti | Fe | C | Mn | S | Si | Al |
% | 38.0-46.0 | 19.5-23.5 | 2.5-3.5 | 1.5-3.0 | 0.6-1.2 | 22.0 min (~33%) | 0.05 max | 1.0 max | 0.03 max | 0.5 max | 0.2 max |
Mechanical properties:
Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
8.14 g/cm3 | 1400 °C (2550 °F) | Psi – 80,000 , MPa – 550 | Psi – 32,000 , MPa – 220 | 30 % |